Summary
Work includes 37,059 gal tack coat, 181,065 SY micro-milling existing pavement (approx 1.10" thru 2.00" thick), material remixing device, smoothness testing, certified inertial profiler, superpave bituminous concrete wearing surface layer, 1/2" maximum aggregate size mix, esal range e, 11,644 Ton superpave bituminous concrete wearing surface layer, widening, 1/2" maximum aggregate size mix, esal range e, 1,103 Ton superpave bituminous concrete upper binder layer, 3/4" maximum aggregate size mix, esal range e, 18,122 Ton superpave bituminous concrete upper binder layer, widening, 3/4" maximum aggregate size mix, esal range e. See attached file.